← Prepreg materials

Porcher Industries

PIPREG

PIPREG · Component prepreg

Matrix system

PA66
PA66

Reinforcement

E-glass
EC6 68 · Woven thermoplastic prepreg

Processing

Thermoforming; compression moulding; autoclave or hot-press consolidation
280.00 °C

Best fit

Aerospace, Automotive, Industrial, Sports, Energy

Construction and composition

FAW
296.80 g/m²
Prepreg areal weight
424.00 g/m²
Resin content
30.00%
Cured ply thickness
Not publicly specified mm

Thermal, storage and handling

Tg: 69.00 °C · Maximum service temperature: 125.00 °C

Storage: 23.00 °C · Shelf life: Not specified months · Out life: Not specified days